Highways Agency Reports
Report Data
| Shelfmark | SSR/TWI/RR16 |
|---|---|
| Author | Francis-Scrutton N |
| Title | Microstructural development in low oxygen weld metal |
| Publisher | The Welding Institute, 1993 |
| Physical Description | ii, 14p., charts, tables |
| Series | Product number 467/1993 |
| Notes | Contents: Introduction; Review of Previous Work; Experimental Procedures; Results; Discussion; Conclusion; Acknowledgements. |
| Keywords | Microalloyed Steels Microstructure O Additions Ti Additions Weld Metal |